ACI PRC-357-24: Design and Construction of Fixed Offshore Concrete Structures - Guide

ACI PRC-357-24: Design and Construction of Fixed Offshore Concrete Structures - Guide

Price: $ 99.00 USD

Choose Product Language

Choose Product Units


Choose Product Format

Description

This document is a guide for the design and construction of fixed reinforced and prestressed concrete structures for service in a marine environment. Only fixed structures that are founded on the seabed are covered.

Contents include materials and durability; dead, deformation, live, environmental, and accidental loads; design and analysis; foundations; construction and installation; and inspection and repair. The two appendixes discuss environmental loads such as wave, wind, and ice loads in detail, and the design of offshore concrete structures for earthquake resistance.

Keywords:

concrete construction; cracking; dynamic loads; earthquakes; earthquake-resistant structures; floating; foundations; gravity-based structure(s); grouting; harbor structures; ice; inspection; marine; offshore structures; platform; post-tensioning; prestressed concrete; slipforming; underwater construction; waves.

 

Document Details

Author: ACI Committee 357

Publication Year: 2024

Pages: 35

ISBN: 9781641952828

Categories: Codes

Formats: Printed Document or Protected PDF/Web View

Table of Contents

CHAPTER 1—GENERAL, p. 2

1.1—Introduction, p. 2

1.2—Scope, p. 2

1.3—Instrumentation, p. 3

1.4—Auxiliary systems and interfaces, p. 3

CHAPTER 2—NOTATION AND DEFINITIONS, p. 3

2.1—Notation, p. 3

2.2—Definitions, p. 3

CHAPTER 3—MATERIALS AND DURABILITY, p. 4

3.1—General, p. 4

3.2—Testing, p. 4

3.3—Prequalification of materials, p. 4

3.4—Quality control, p. 4

3.5—Durability, p. 4

3.6—Cementitious materials, p. 5

3.7—Mixing water, p. 5

3.8—Aggregates, p. 5

3.9—Chemical admixtures, p. 6

3.10—Concrete, p. 6

3.11—Reinforcing steel, p. 7

3.12—Prestressing steel, p. 8

3.13—Fiber reinforcement, p. 9

3.14—Grout for underbase, p. 9

3.15—Anchorages for embedments and connections to steel work, p. 9

3.16—Electrical ground, p. 9

3.17—Durability of pipes containing pressure, p. 9

3.18—Epoxy resins, p. 9

3.19—Formwork, p. 10

CHAPTER 4—LOADS, p. 10

4.1—General, p. 10

4.2—Load categories, p. 10

4.3—Design phases, p. 10

4.4—Limit states and load combinations, p. 11

4.5—Interfaces among various disciplines, p. 11

CHAPTER 5—DESIGN AND ANALYSIS, p. 11

5.1—General, p. 11

5.2—Strength, p. 11

5.3—Serviceability, p. 11

5.4—Design considerations, p. 12

5.5—Special requirements, p. 13

5.6—Other strength requirements, p. 15

5.7—Structural analysis, p. 16

CHAPTER 6—FOUNDATIONS, p. 17

6.1—Site investigation, p. 17

6.2—Sea floor stability, p. 19

6.3—Scour, p. 19

6.4—Design of shallow foundations, p. 19

6.5—Skirt piles, p. 20

CHAPTER 7—CONSTRUCTION, INSTALLATION, AND RELOCATION, p. 21

7.1—General, p. 21

7.2—Buoyancy and floating stability, p. 21

7.3—Construction joints, p. 22

7.4—Concreting in hot or cold weather, p. 22

7.5—Curing of concrete, p. 22

7.6—Reinforcement, p. 22

7.7—Prestressing tendons, ducts, and grouting, p. 23

7.8—Initial floatation, p. 23

7.9—Construction while afloat or temporarily grounded, p. 23

7.10—Towing, p. 23

7.11—Installation, p. 24

7.12—Construction on site, p. 24

7.13—Connection of adjoining structures, p. 25

7.14—Prevention of damage due to freezing, p. 25

7.15—Relocation, p. 25

CHAPTER 8—INSPECTION AND REPAIR, p. 25

8.1—General, p. 25

8.2—Inspection, p. 25

8.3—Repair of concrete, p. 26

8.4—Repairs of cracks, p. 26

CHAPTER 9—REFERENCES, p. 26

Authored documents, p. 28

APPENDIX A—ENVIRONMENTAL LOADS, p. 29

A.1—Introduction, p. 29

A.2—Wave loads, p. 29

A.3—Wave diffraction, p. 30

A.4—Currents, p. 30

A.5—Design wave analysis, p. 30

A.6—Wave response spectrum analysis, p. 30

A.7—Dynamic response analysis, p. 30

A.8—Wind loads, p. 31

A.9—Ice/iceberg loads, p. 31

A.10—Earthquakes, p. 31

APPENDIX B—DESIGN FOR EARTHQUAKES, p. 31

B.1—Introduction, p. 31

B.2—Overall design procedure, p. 32

B.3—Seismicity study, p. 32

B.4—Site response studies, p. 32

B.5—Selection of design criteria, p. 32

B.6—Dynamic analysis, p. 33

B.7—Stress analysis, p. 34

B.8—Failure modes, p. 34

B.9—Ductility requirements, p. 34

B.10—Proper reinforcement detailing, p. 35

B.11—Other factors, p. 35

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).