ACI SPEC-351.5-24: Epoxy Grout Installation between Foundations and Equipment Bases—Specification

ACI SPEC-351.5-24: Epoxy Grout Installation between Foundations and Equipment Bases—Specification

Currency Display

Your Price:$ 54.00 USD

Member Price: $ 34.00 USD

Save $ 20.00 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Description

This Specification covers minimum requirements for installing epoxy grouting between foundations and equipment bases. Included are requirements for materials, placement, forming, testing, repair, and quality control. A mandatory requirements checklist and an optional requirements checklist are provided to assist the Architect/Engineer in supplementing the requirements of this Specification as required or needed by designating or specifying individual project requirements.

Keywords:

cement grout; cementitious grout; epoxy grout; equipment grout; foundations; grout.

 

Document Details

Author: ACI Committee 351

Publication Year: 2024

Pages: 7

ISBN:

Categories: Codes, Grouting, Specifications

Formats: Printed Document or Protected PDF/Web View

Table of Contents

PART 1—GENERAL, p. 2

1.1—Scope, p. 2

1.2—Interpretation, p. 2

1.3—Definitions, p. 2

1.4—Referenced standards, p. 3

1.5—Submittals, p. 3

1.6—Delivery, storage, and handling, p. 3

1.7—Quality assurance and control, p. 3

1.8—Acceptance of Work, p. 3

PART 2—PRODUCTS, p. 4

2.1—Materials, p. 4

2.2—Accessories, p. 4

PART 3—EXECUTION, p. 4

3.1—Preparation, p. 4

3.2—Installation, p. 5

3.3—Testing and inspection, p. 6

3.4—Repair, p. 6

3.5—Cleaning, p. 6

3.6—Hot weather curing, p. 6

NOTES TO SPECIFIER, p. 6

General notes, p. 6

Forward to checklists, p. 6

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).