325.3R-85: Guide for Design of Foundations and Shoulders for Concrete Pavements

325.3R-85: Guide for Design of Foundations and Shoulders for Concrete Pavements

Currency Display

Your Price:$ 21.50 USD

Member Price: $ 14.00 USD

Save $ 7.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**WITHDRAWN DOCUMENT - This document has been discontinued by ACI and is available for informational purposes only.

Description

Methods are suggested for material selection, moisture control, and compaction or treatment of soils and materials to assure volume stability and uniform support for concrete pavements. Various environments are considered and appropriate methods of subgrade preparation outlined. Base and subbase functions are defined and adaptability of types of subbases discussed.

 

Document Details

Author: ACI Committee 325

Publication Year: 2017

Pages: 8

ISBN:

Categories: Pavements

Formats: PDF

This document is Withdrawn

Table of Contents

Chapter 1 - Introduction

1.1 -- General

Chapter 2 - Definitions

2.1 -- General

Chapter 3 - Subgrades and embankments

3.1 -- General

3.2 -- Preparation of subgrade

Chapter 4 - Subbases

4.1 -- General

4.2 -- Types of subbases

4.3 -- Design and location

Chapter 5 - Shoulders

5.1 -- General considerations

Chapter 6 - Evidence of foundation settlement

6.1 -- Design field survey

Chapter 7 -- Pumping

7.1 -- Pumping considerations

Chapter 8 -- Joint faulting

8.1 -- Causes

Chapter 9 -- High joints

9.1 -- General

Chapter 10 -- Cracking

10.1 -- Causes and locations of cracks

Chapter 11 - Pavement breaks and settlements

11.1 -- Causes and treatments

Chapter 12 - Undulations

12.1 -- Causes

Chapter 13 - Soil report

13.1 -- General

Chapter 14 - References

14.1 -- Recommended references

14.2 -- Cited references

14.3 -- Additional references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).