ACI PRC-308-213-13 Report on Internally Cured Concrete Using Prewetted Absorptive Lightweight Aggregate

Currency Display

Your Price: $ 56.50 USD

Member Price: $ 36.00 USD

Save $ 20.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Notes/Preview

Preview

Description

This report introduces the concepts of and describes the process benefit and applications for using prewetted lightweight aggregate to increase cement hydration in internally cured concrete. It also describes mixture proportioning and absorptive material selection and discusses the benefits relating to sustainability. The materials, processes, quality control measures, and inspections described should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI certifications or equivalent.

Keywords: absorption; curing; desorption; durability; high-performance concrete; hydration; internal curing; internally cured concrete; lightweight aggregate; outside curing; permeability; saturated-surface-dry; shrinkage; strength; supplementary cementitious materials; water movement.

 

Document Details

Author: ACI Committees 308, 213

Publication Year: 2013

Pages: 12

ISBN: 9780870318214

Categories: Curing

Formats: PDF, ePub, or Kindle

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1—Introduction

1.2—Scope

CHAPTER 2—NOTATION AND DEFINITIONS

2.1—Notation

2.2—Definitions

CHAPTER 3—PROCESS

3.1––General

3.2—Justification

3.3—Water movement

3.4—Autogenous shrinkage and self-desiccation

3.5—Mechanism of internal curing

3.6—Water movement during hydration observed using X-ray microtomography

CHAPTER 4—INTERNALLY CURED CONCRETE (ICC): EFFECTS, BENEFITS, AND APPLICATIONS

4.1—Early-age shrinkage reduction

4.2—Crack reduction

4.3—Compressive strength

4.4—Overdosing prewetted lightweight aggregate (PLA)

4.5—Flexural strength

4.6—Mitigation of warping and dimensional stability

4.7—Modulus of elasticity

4.8—Permeability and resistance to deicing chemicals

4.9—Creep

4.10—Durability

CHAPTER 5—BATCHING PROCEDURES

5.1—Choice of absorptive material

5.2—Mixture proportioning using absorptive materials

5.3—Prewetting lightweight aggregate

5.4—Concrete batching. Mixing, transporting, placing, and finishing

CHAPTER 6—SUSTAINABLE CONCRETE CONSTRUCTION USING INTERNALL CURED CONCRETE (ICC)

CHAPTER 7—REFERENCES

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.