222.1-96: Provisional Standard Test Method for Water-Soluble Chloride Available for Corrosion of Embedded Steel in Morta

222.1-96: Provisional Standard Test Method for Water-Soluble Chloride Available for Corrosion of Embedded Steel in Morta

Currency Display

Your Price:$ 19.50 USD

Member Price: $ 14.00 USD

Save $ 5.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**WITHDRAWN DOCUMENT - This document has been discontinued by ACI and is available for informational purposes only.

Description

Some water-soluble chlorides, primarily in certain aggregates, do not induce corrosion of embedded reinforcing steel since these chlorides are bound within the aggregate. Currently, available test methods cannot distinguish between water-soluble chlorides that support corrosion and those that do not. This test method provides procedures for the sampling and analysis of hydraulic-cement mortar, concrete, or aggregate for chloride which is water-soluble and contributes to the corrosion of reinforcing steel.

Keywords: Water-soluble chlorides; corrosion; steel; mortar; concrete; Soxhlet Extractor.

 

Document Details

Author: ACI Committee 222

Publication Year: 2017

Pages: 3

ISBN:

Categories: Testing

Formats: PDF

This document is Withdrawn

Table of Contents

Section 1 - Scope

Section 2 - Significance and Use

Section 3 - Apparatus

Section 4 - Reagents

Section 5 - Sampling

Section 6 - Sample Preparation

Section 7 - Procedure

Section 8 - Calculation

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).