306R-10 Guide to Cold Weather Concreting

306R-10 Guide to Cold Weather Concreting

Currency Display

Your Price:$ 74.00 USD

Member Price: $ 74.00 USD

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**A newer version of this document exists**

NEW VERSION

 

Description

The objectives of cold weather concreting practices are to prevent damage to concrete due to freezing at early ages, ensure that the concrete develops the required strength for safe removal of forms, maintain curing conditions that foster normal strength development, limit rapid temperature changes, and provide protection consistent with the intended serviceability of the structure.

Concrete placed during cold weather will develop sufficient strength and durability to satisfy intended service requirements when it is properly produced, placed, and protected. This guide provides information for the contractor to select the best methods to satisfy the minimum cold weather concreting requirements.

This guide discusses: concrete temperature during mixing and placing, temperature loss during delivery, preparation for cold weather concreting, protection requirements for concrete that does not require construction supports, estimating strength development, methods of protection, curing requirements, and admixtures for accelerating setting and strength gain including antifreeze admixtures. The materials, processes, quality control measures, and inspections described in this document should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI Certifications or equivalent.

Keywords: accelerating admixtures; antifreeze admixtures; cold weather concreting; concrete temperature; curing; enclosures; form removal; freezing and thawing; heaters; heating aggregates; insulating materials; maturity testing; protection; strength development.

 

Document Details

Pages: 26

Categories: Codes

Formats: Protected PDF/Web View

This document is Historical

Table of Contents

Chapter 1—Introduction

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—Objectives, principles, and economy

3.1—Objectives

3.2—Principles

3.3—Economy

Chapter 4—General requirements

4.1—Planning

4.2—Protection during unexpected freezing

4.3—Concrete temperature

4.4—Temperature records

4.5—Heated enclosures

4.6—Finishing air-entrained slabs

4.7—Concrete workability

Chapter 5—Temperature of concrete as mixed and placed, and heating of materials

5.1—Placement temperature

5.2—Mixing temperature

5.3—Heating mixing water

5.4—Heating aggregates

5.5—Steam heating of aggregates

5.6—Overheating of aggregates

5.7—Calculation of mixture temperature

5.8—Temperature loss during delivery

Chapter 6—Preparation before concreting

6.1—Preparation of surfaces in contact with fresh concrete

6.2—Massive metallic embedments

6.3—Subgrade condition

Chapter 7—Protection against freezing and protection for concrete not requiring construction supports

7.1—Protection methods

7.2—Protection period

7.3—Protection for strength gain

7.4—Temperature drop after removal of protection

7.5—Allowable temperature differential during stripping

Chapter 8—Protection for structural concrete requiring construction supports

8.1—Introduction

8.2—Field-cured cylinders

8.3—In-place testing

8.4—Maturity testing

8.5—Attainment of design strength

8.6—Increasing early strength

8.7—Cooling of concrete

8.8—Estimating strength development

8.9—Removal of forms and supports

8.10—Specification recommendations

8.11—Estimating strength development—modeling of cold weather placements

Chapter 9—Equipment, materials, and methods of temperature protection

9.1—Introduction

9.2—Insulating materials

9.3—Selection of insulation when supplementary heat is not used

9.4—Selection of insulation for use with hydronic heaters

9.5—Heaters

9.6—Enclosures

9.7—Internal heating

9.8—Temperature monitoring

9.9—Temporary removal of protection

9.10—Insulated forms

Chapter 10—Curing requirements and methods

10.1—Introduction

10.2—Curing during the protection period

10.3—Curing following the protection period

Chapter 11—Acceleration of setting and strength development

11.1—Introduction

11.2—Accelerating admixtures

11.3—Rapid-setting cements

Chapter 12—References

12.1—Referenced standards and reports

12.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).