Table of Contents 
                        Preface
Chemical Admixtures
SP-229—1: Chloride-Free Accelerators for Concrete Setting and Hardening
by H. Justnes
Deformations, Creep, and Cracking Control
SP-229—2: Realkalisation of the Carbonated Concrete using Alkaline Solutions
by F.W.C. Araújo and E.J. Pazini Figueiredo
SP-229—3: Effects of Binder Materials on the Properties of Polystyrene Aggregate Concrete
by R. Sri Ravindrarajah, V. DiFalco, and S. Surian
SP-229—4: Predicting Long-Term Creep from Short-Term Creep Test
by V. Sirivivatnanon
SP-229—5: Self Consolidating Concrete, High-Performance and Normal Concrete Affected by Creep at Different Age, Curing, Load Level, Strength, and Water-Cement Ratio with some Interrelated Properties
by B. Persson
Durability
SP-229—6: Influence of Chemical Activation on Chloride Penetration in Concrete
by A.L.G. Gastaldini, G.C. Isaia, N.S. Gomes, and J.E.K. Sperb
SP-229—7: The Rehabilitation Method of Electrochemical Chloride Extraction by an Engineering View 1
by E. Monteiro, P. Helene, and A. Carneiro
SP-229—8: Sorptivity: Parameter for the Evaluation of Cover Concrete Quality 1
by V.L. Taus, A.A. Di Maio, and L.P. Traversa
SP-229—9: Evaluation of Cover Concrete by Analysis of Chloride Diffusion Coefficients
by O. Cascudo, H. Carasek, M.-P. Yssorche-Cubaynes, A.N. Lopes, and J.-P. Ollivier
SP-229—10: Advanced Methods of Corrosion Measurement in Real Concrete Structures 1
by C. Andrade and I. Martinez
SP-229—11: Application of Different Curing Procedures in High-Performance Concrete (HPC)
by R. de Oliveira Pinto, A.L.B. Geyer, and A. Liduário
SP-229—12: Diffusion of Chloride Ions in Unsaturated Concrete: Forecast of Service Life in a Wet-Dry Environment
by A.T.C. Guimarães and P.R.L. Helene
SP-229—13: Carbonation-Induced Corrosion in Buildings Under Tropical Environments
by E.I. Moreno and R. Solis-Carcaño
SP-229—14: Behavior of Juxtaposed Galvanic Couples in Small Repaired Beams by Using Primers to the Reinforcement
by P. Castro-Borges, C. Andrade, C. Alonso, and E. Pazini Figueiredo
SP-229—15: The Influence of Biodeterioration on Concrete Durability
by S.M.M. Pinheiro, M.R. Silva, and F.L. dos Santos Souza
SP-229—16: Durability of 15-year Old Concrete with Surface Coating Materials under Marine Environment
by T. Yamaji, K.-I. Komure, and H. Hamada
SP-229—17: A New Construction Material—Non-Corrosive Basalt Bar Reinforced Concrete
by V. Ramakrishnan and R.K. Panchalan
Fiber Concrete
SP-229—18: Theoretical Model for Confined Steel-Fiber-Reinforced High-Strength Concrete
by H.C. Lima, Jr. and J.S. Giongo
Fire Resistance
SP-229—19: Microstructural Changes in High and Ultra High Strength Concrete Exposed to High Temperature Environments
by C. Alonso, C. Andrade, E. Menendez, and E. Gayo
Nondestructive Tests
SP-229—20: Methodology for the Structural Assessment of Concrete Affected by Reinforcement Corrosion
by J. Rodriguez, L.M. Ortega, J. Aragoncillo, D. Izquierdo, and C. Andrade
SP-229—21: Evaluation of the Compressive Strength of Concrete by Different Nondestructive Methods
by A.C.J. Evangelista, I.A.E.M. Shehata, and L.C.D. Shehata
Quality Control
SP-229—22: Statistical Measures of HPC Compressive Strength
by S.F. Freyne, W.M. Hale, and B.W. Russell
Structural Behavior
SP-229—23: Comparative Evaluation of Flexural Fatigue Behavior of High-Volume Fly Ash and Plain Concrete
by V. Ramakrishnan, V.M. Malhotra, and W.S. Langley
Strengthening of Structures
SP-229—24: Cyclic Shear Behavior of Connection between Precast Beam and Deck with Steel Fiber-Reinforced Concrete
by D.L. Araújo and M.K. El Debs
SP-229—25: Behavior of Reinforced Concrete Slabs Strengthened in Flexure by Concrete Overlays
by J.M. Calixto, E.F. Pires, S.A. Lima, and E.M. Piancastelli
Supplementary Cementing Materials
SP-229—26: Rice Husk Ash with Low Carbon Content
by S. Santos and L.R. Prudêncio, Jr.
SP-229—27: The Influence of Silica Fume on the Apparent Activation Energy of HPC Mixtures
by M.P. Barbosa, R.C.A. Pinto, and L.D.P. Peres
SP-229—28: Effects of Alkali-Activation of Slag Concrete
by M.A.M. Coelho, M.G. da Silva, F.L. dos Santos Souza, R. Sarmento, R.P. de Moraes Frasson, S.M. de Moraes Pinheiro, E. Zandonade, and T. Morimoto
SP-229—29: Properties of Steam Cured Concretes with Silica Fume Addition
by P.S. Bardella and G. Camarini
SP-229—30: Bottom Ash from Municipal Solid Waste from Incineration Plants as Mineral Additions for Concrete
by L. Bertolini, M. Carsana, D. Cassago, M. Collepardi, and A.Q. Curzio
Sustainability
SP-229—31: Polymeric Admixtures as Bonding Agent between Tire Rubber and Concrete Matrix
by A.C. de Albuquerque, N.P. Hasparyk, M.A.S. Andrade, and W.P. de Andrade
SP-229—32: Properties of Concrete with Recycled Concrete Coarse Aggregates
by A.M. Buttler and E.F. Machado, Jr.