Table of Contents 
                        -How to Make Concrete That Will be Immune to the Effects 
    of Freezing and Thawing, by B. Mather
-Durability of High Strength Concrete, by P.K. Mehta
-Deicer Salt Scaling Resistance of High Performance 
    Concrete, by R. Gagne, M. Pigeon, and P.-C. Aitcin
-Suitability of the Measurement Techniques of Oxygen
    Permeability in Order to Predict Corrosion Rates of 
    Concrete Rebars, by C. Andrade, C. Alonso, 
    I. Rz-Maribona, and M. Garcia
-Freeze-Thaw Durability of Concrete Coated with Linseed
   Oil, by T. Rezansoff and D. Scott
-Effects of "Second-Generation" High Range Water-
   Reducers on Durability and Other Properties of Hardened 
   Concretes, by D. Whiting and W. Dziedzic
-Air Voids in Concrete: A Study of the Influence of 
   Superplasticizers by Means of Scanning Electron 
   Microscopy and Optical Microscopy, by R. Pleau,
   M. Pigeon, R.M. Faure, and T. Sedran
-High Quality Tremie Concretes for Underwater Repairs, 
   by K.H. Kyayat, B.C. Gerwick, Jr., and W.T. Hester
-Corrosion of Reinforcing Steel in Concrete Exposed to 
   Marine and Freshwater Environments, by S. Somayaji, 
   D. Keeling, and R. Heidersbach
-Long Service Life of Concrete, by L.H. Tuthill
-The Freezing-and-Thawing Environment: What is Severe?, 
    by N.M. Vanderhors and D.J. Janssen
-Field Exposure of Concrete to Severe Natural Weathering, 
    by J.F. Lamond and M.K. Lee
-Freeze-Thaw Durability and Deicer Salt Scaling Resistance
    of Roller Compacted Concrete Pavements, by J. Marchand, 
    M. Pigeon, H.L. Isabelle, and J. Boisvert
-An Overview of a New Field and Laboratory Study of the 
    Durability of Reinforced and Post-Tensioned Concrete 
    in the Marine Environment, by E.F. O'Neil, D.V. Reddy, 
    T.W. Bremner, W.H. Hartt, and M. Arockiasamy
-The Effects of Calcium Nitrite and Microsilica Admixtures 
    on Corrosion Resistance of Steel in Concrete, by N.S. Berke 
    and K.M. Sundberg
-Potential for Carbondation of Concrete in Canada, by
    J.A. Bickley
-Involvement of Sulfur-Oxidizing Bacteria in Concrete 
    Deterioration, by C.F. Kulpa and C.J. Baker
-Repair Strategy and Evaluation of Materials and Methods for
    Rehabilitation of Concrete Shells for Two Natural Draft Cooling
    Towers, by S. Gebler, P. Nussbaum, W. Dziedzic, J. Glikin, 
    A. Litvin, W. Bilenki, Jr., and J. Stefanik
-Durability of a Precast Prestressed Concrete Conveyor Bridge 
    Structure at a Salt Mine After 17 Years of Service, by
    R.W. Poston and M. Schupack
-Rehabilitation of Great Lakes Steel's Number One Dock, 
    by C.J. Hookham
-Deterioration and Rehabilitation of the Elevated Roadway 
    Bridge at Baltimore/Washington International Airport, by
    A.M. Vaysburd
-Evaluation and Repair of Concrete Structuree in Urban 
    Environment: Case Study, by D. Bjegovic, V. Ukraincik, 
    and Z. Beus
-Evaluation of Reinforced Concrete Masonry in a Highly Corrosive
    Environment, by D.J. Akers
-Performance of Concrete in a High Chloride-Sulfate Environment,
    by M. Maslehuddin, H. Saricimen, A.I. Al-Mana, and M. Shamim