Description 
                            This Specification covers methyl methacrylate slurry (MMS) overlays for bridge and parking garage decks. Type MMS polymer overlay incorporates methyl methacrylate-based primer, binder, and top coat with selected filler and aggregate to produce a flexible, skid-resistant, and water-resistant slurry overlay. The overlay is used for both new construction and rehabilitation. The overlay is placed by applying the polymer slurry system to the surface and broadcasting aggregate. This Specification includes requirements for chemical components, aggregates, storage and handling, surface preparation, surface profile, mixing, placement, finishing, and quality control. The materials, processes, quality control measures, and inspections described in this document should be tested, monitored, or performed as applicable only by individuals with appropriate ACI certifications or equivalent.
Keywords: aggregate; bridge decks; methyl methacrylate; mortar; overlays; parking garage decks; polymer; premixed; resin; slurry.
                        
                    
                
                
                        Table of Contents 
                        Section 1—General
1.1—Scope
1.2—Definitions
1.3—Reference standards
1.4—Submittals
1.5—Project conditions
1.6—Labeling, storage, and handling of materials
1.7—Safety
Section 2—Products
2.1—Methyl methacrylate-based primer
2.2—Methyl methacrylate-based binder
2.3—Filler
2.4—Methyl methacrylate-based top coat
2.5—Aggregate
2.6—Polymer overlay slurry
Section 3—Execution
3.1—Procedure qualification
3.2—Surface preparation
3.3—Mixing methyl methacrylate-based primer, binderfiller
slurry, and top coat
3.4—Overlay application
3.5—Curing
3.6—Excess aggregate removal
3.7—Joints
3.8—Opening to traffic
Notes to Specifier
General notes
Foreword to checklists
Mandatory Requirements Checklist
Submittals Checklist
                    
                
                
                    
                        Return/Exchange Policy 
                        Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
                        Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
                        Subscriptions These items are not eligible for return.
                        Exchanges:  Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).