Effect of High-Strength Concrete Columns on the Behavior of Slab-Column Connections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of High-Strength Concrete Columns on the Behavior of Slab-Column Connections

Author(s): H. Marzouk, Mohamed Emam, and M. Sameh Hilal

Publication: Structural Journal

Volume: 93

Issue: 5

Appears on pages(s): 545-554

Keywords: columns (supports); crack width and spacing; ductility; energy absorption; failure mechanisms; high-strength concretes; moments; slabs; stiffness; strains.

DOI: 10.14359/9713

Date: 10/1/1996

Abstract:
Current code provisions for the design of slab-column connections are based on the test results of connections constructed with relatively low compressive strengths not exceeding 40 MPa. Hence, further investigations are needed to develop and evaluate more research data to determine whether the code requirements are realistic and adequate for high-strength concrete at levels considerably higher than 40 MPa. Results of tests conducted on seven interior slab-column connections (75 to 85 MPa) and normal-strength concrete slabs (30 to 40 MPa) are evaluated for use in the design of slab-column connections. The variables selected for this study are strength of concrete, flexural steel reinforcement ratio, and moment-to-shear ratio. It has been found that the use of high-strength columns increased con-nection shear strength compared to normal-strength concrete by about 5 percent in the case of no moment and 17 percent in the case of high moment. Not only was shear strength increased but the connection perfor-mance was greatly enhanced by the use of high-strength concrete columns.