Title: Segmental Box-Girder Bridge construction

Author(s): M. K. Hurd

Publication: Concrete International

Volume: 8

Issue: 9

Appears on pages(s): 19-27

Keywords:

DOI:

Date: 9/1/1986

Abstract:
Gives an overall background for understanding the construction alternatives available for segmental box-girder construction, including cast-in-place and precast segmental construction, as well as principal methods of erection. These are balanced cantilever, progressive placing, incremental launching, and span-by-span erection.




  