International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guide to the Design of Anchor Bolts Other Steel Embedments

Author(s): R.W. Cannon, D. A. Godfrey and F. L.,Moreadith

Publication: Concrete International

Volume: 3

Issue: 7

Appears on pages(s): 28-41

Keywords: anchorage (structural); anchor bolts; an-& 0’S ( fasteners); building codes; composite con struction (concrete and steel); embedment; grouting; inserts; loads (forces); reinforced concrete; shear properti es structural design; studs.

DOI:

Date: 7/1/1981

Abstract:
There has been little published on the design of steel embedments. Many designers looking for guidance have found the work of ACI Committee 349, Concrete Nuclear Structures, extremely helpful. Because there may be designers who are not aware of this information, which is an appendix to the Code prepared by Committee 349, a modified version is offered here which can be applied outside the design of nuclear structures.




  