Title: Tests of Masonry Cements
Author(s): George W. Washa
Publication: Journal Proceedings
Volume: 40
Issue:
Appears on pages(s): 165-172
Keywords:
Date: 11/1/1943
Abstract:
Presents results of tests made on seven masonry cements. Properties reported are: water retention, water repellency, tensile and compressive strength, linear chanaes due to autoclavinq and to three different storage conditions. Strength and linear change properties are reported to 5 years.