Abstract:
Shortage of steel for reinforcement was the immediate incentive for this report which is intended to guide the designer in the use of unreinforced concrete for suitable applications. It discusses the quality of concrete, volume changes, and recommends allowable stresses as a basis for discussion and -with due cautions for immediate use in conjunction with Building Regulations for Reinforced Concrete (AC1 318-41).




  