Title: Methods of Handling and Placing Concrete at Shasta Dam

Author(s): C. S. Rippon

Publication: Journal Proceedings

Volume: 39

Issue:

Appears on pages(s): 1-8

Keywords:

Date: 9/1/1942

Abstract:
Describes briefly equipment and methods employed by contractors in handling and placing 6,500,OOO cu yd of concrete in construction of Shasta Dam and power plant.




  