Title: Concrete Exposed To Sulphur Water

Author(s): John S. Nelles

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 441-452

Keywords: none

Date: 2/1/1941

Abstract:
Progress report on The Detroit Edison Co. tests showing the condition of concrete specimens comprising different mixes, admixtures, and cements, after I2 years exposure completely submerged in flowing sulfur water. The data include compressive strength curves and extent of disintegration, from which some conclusions have been drawn and some recommenda- tions made.




  