Contrasts practices in form construction for structural and architectural concrete. Discusses materials acceptable for contact surfaces, choice of woods or plywoods, and grades of lumber for effects desired Describes correct practices in erection of forms back: ing, bracing, nails, ties, preparation of forms, rate of placing concrete, necessary for form construction joints, and provisions illustrated. removal. Numerous form details




  