Title: Remarks On Durability Of Concrete

Author(s): Roy W. Carlson

Publication: Journal Proceedings

Volume: 35

Issue: 4

Appears on pages(s): 359-364

Keywords: none

Date: 4/1/1939

Abstract:
A statement of factors affecting the durability of concrete; the fatigue action of volume changes pro duced by changes in temperature and moisture; the freezing of water in the pores of concrete; the phenomenon of bleeding; the thermai, elastic, and hygral properties of the constituents of concrete. Emphasis is placed on the need for test methods. which will permit more accurate prediction of durbiity.




  