Abstract:
The vacuum process provides a practical means of obtaining concrete with minimum water-cement ratio. It removes unwanted mixina water from the concrete after it has been placed in the forms, Process is described, and application to floors. walls. bridge decks, and various projects are enumerated. ‘urfacing and resurfacing




  