Title: The Effect Of Vibration On The Strength And Uniformity Of Pavement Concrete

Author(s): F. H. Jackson and W. F. Kellermann

Publication: Journal Proceedings

Volume: 33

Issue: 3

Appears on pages(s): 411-432

Keywords: none

Date: 3/1/1937

Abstract:
Tests were made on full size pavement slabs, using regular construction equipment. Several well-known types of high frequency surface vibrators were in-vestigated. Major indications were (I ) that with equal cement contents, vibration increased flexural strength about IO percent, (2) that, with equal water-cement ratios, vibration effected a saving in cement of about IO percent and (3) that the uni-formity of pavement concrete of l-in. slump was markedly improved by the application of surface vi bration.




  

Please enter this 5 digit unlock code on the web page.