Title: Some Comparisons Of European And American Concrete Practice

Author(s): F. R. McMillan

Publication: Journal Proceedings

Volume: 33

Issue: 3

Appears on pages(s): 395-410

Keywords: none

Date: 3/1/1937

Abstract:
Illustrated descriptions are given of various typical European structures including bridges, dams, and water tanks.




  