Title: Cold Weather protection Of Concrete
Author(s): R. B. Young and Wilfrid Schnarr
Publication: Journal Proceedings
Volume: 30
Issue: 3
Appears on pages(s): 292-304
Keywords: none
Date: 3/1/1934
Abstract:
It is not difficult nor expensive to provide satisfactory curing conditions for concrete in cold weather. Success depends on simple precautions and careful planning. The authors outline correct techniques considered and list precautions that must be considered.