Reinforced Concrete Column Investigation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reinforced Concrete Column Investigation

Author(s): ACI Committee 105

Publication: Journal Proceedings

Volume: 28

Issue: 11

Appears on pages(s): 157-158

Keywords: none

DOI: 10.14359/8233

Date: 11/1/1931

Abstract:
The third progress report of Committee 105 introduces the reports from Lehigh University and the University of I ll inoi s Series 7 in the column investigation program.




  