Title: Shore And Storm Protection On The Gulf Coast

Author(s): J.B. Converse

Publication: Journal Proceedings

Volume: 26

Issue:

Appears on pages(s): 626-636

Keywords: none

Date: 4/1/1930

Abstract:
A review of conditions to be encountered on the Gulf Coast due to tropical hurricanes and the manner in which they have been met in building structures to prevent beach erosion and the flooding of populated areas.




  