Title: Some Tests Of Concrete Masonry Units Cured With High Pressure Steam

Author(s): P. M. Woodsworth

Publication: Journal Proceedings

Volume: 26

Issue:

Appears on pages(s): 504-512

Keywords: none

Date: 2/1/1930

Abstract:
The main purpose of this investi data concerning the effect of h gation was to obtain iqh-pressure steam curing on (I) early strength, (2) ultimate strength, and (3) strenqth as affected bv time interval between molding and -curing. The author believes that hi pressure steam curing has possibilities as a means f h- or developing concrete p rod u c t s having high early strength and low shrinkage.




  