Title: Variations in Standard Portland Cements

Author(s): P. H. Bates

Publication: Journal Proceedings

Volume: 26

Issue:

Appears on pages(s): 65-95

Keywords: none

Date: 11/1/1929

Abstract:
Discusses the variations in commercial portland cements as reflected by variations in their early and late strength, permeability, workability building stone, shrinkage, plastic yield, in reaction with heat of hydration, reactions to curing conditions, and color of concrete.




  