Title: Trends in Concrete Pavement Design

Author(s): Harry D. Cashell

Publication: Journal Proceedings

Volume: 60

Issue: 4

Appears on pages(s): 501-514

Keywords:

DOI: 10.14359/7865

Date: 4/1/1963

Abstract:
While there is a great deal of variety in the United States in the design of concrete highway pavements, there have been trends toward uniformity that can be noted. Among the items where a trend toward uniformity has been noticed are: subbase requirements, pavement cross sections, pavement types, slab lengths, and joining practices.




  