ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Performance of Bonded Concrete Overlays

Author(s): Roy W. Gillette

Publication: Journal Proceedings

Volume: 60

Issue: 1

Appears on pages(s): 39-50

Keywords:

DOI: 10.14359/7841

Date: 1/1/1963

Abstract:
A number of bonded overlays using portland cement grout have been employed in resurfacing pavements since 1954. This paper presents results of a survey on a number of these pavements to ascertain the performance of the overlays. The overlays were sounded and their surfaces inspected visually. Cores were taken to confirm areas of bond distress. Some of the specific projects surveyed are described. The introduction to the paper outlines some of the more important published material on the proper methods and techniques of bonding new concrete surfaces to old concrete surfaces.




  

Please enter this 5 digit unlock code on the web page.