Title: Chimney Foundation

Author(s): John W. Smith and Max Zar

Publication: Journal Proceedings

Volume: 61

Issue: 6

Appears on pages(s): 673-700

Keywords:

DOI: 10.14359/7802

Date: 6/1/1964

Abstract:
A method is described for designing chimney foundations for various loading conditions with the help of circular slab theory. Pile foundations are included. Charts are presented for facilitating the analysis. An example given for a footing on soil.




  