Title: Creep of Concrete at Elevated Temperatures

Author(s): Karim W. Nasser and Adam M. Neville

Publication: Journal Proceedings

Volume: 62

Issue: 12

Appears on pages(s): 1567-1580

Keywords: compressive strength, concrete, creep, high temperature, modulus of elasticity, pressure vessel, research, stress-strength ratio, temperature.

Date: 12/1/1965

Abstract:
Data on creep of concrete, both mass- and water-cured in the temperature range 70 to 205 F are presented, together with results of subsequent creep recovery tests. Hence, observations on the viscous character of the creep deformation are made. Data on strength and elasticity of one mix within the same termperature range are presented.




  