Title: Method of Estimating Creep of Concrete When the Stress-Strength Ratio Varies With Time

Author(s): Adam M. Neville and Michael M. Staunton

Publication: Journal Proceedings

Volume: 62

Issue: 10

Appears on pages(s): 1293-1312

Keywords: concrete, creep, design, research, stress-strength ratio, time

Date: 10/1/1965

Abstract:
Analytical and numerical methods are presented for the computation of creep of concrete when the stress-strength ratio varies with time. The computations are based on a standard creep curve for a concrete of constant strength.




  