Shear Strength of Concrete Deep Beams under Fatigue Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Concrete Deep Beams under Fatigue Loading

Author(s): Susanto Teng, Wei Ma, and Fang Wang

Publication: Structural Journal

Volume: 97

Issue: 4

Appears on pages(s): 572-580

Keywords: beams; crack deflection; shear strength; web reinforcement

DOI: 10.14359/7423

Date: 7/1/2000

Abstract:
This paper presents an experimental investigation involving 12 reinforced concrete deep beams subjected to fatigue loading. Three different arrangements of web reinforcement were considered, namely: without web reinforcement, with vertical web reinforcement only, and with inclined web reinforcement. The tests revealed that the arrangements of web reinforcements have significant influence on the structural response of deep beams under fatigue loading. With load repetitions, the midspan deflection and maximum crack width increased, while the shear strength decreased. The investigation also showed that the relevant ACI equations can be applied to deep beams under fatigue or repeated loading once the properties of the concrete and the reinforcement are adjusted to take account of the effect of fatigue loading.