Special Techniques for Producing High Strength Concrete

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Special Techniques for Producing High Strength Concrete

Author(s): Cameron MacInnis and Donald V. Thomson

Publication: Journal Proceedings

Volume: 67

Issue: 12

Appears on pages(s): 996-1002

Keywords: admixtures; compressive strength; concretes; fly ash; high strength concretes; mixing; mixing time; mortars (material) ; research; slurries; vibration; water-cement ratio; water-reducing agents.

Date: 12/1/1970

Abstract:
Three special techniques (high speed slurry mixing, seeding, and revibration) and two admixtures (fly ash and lignosulfonic acid water-reducing agent were employed in a research program designed to produce high compressive strength concretes in the range of 6000 to I 1,000 psi (420 to 770 kg/cm2). The water-reducing agent, high speed slurry mixing, and revibration, appear to hold the most promise for increasing the compressive strength of concrete in this strength range. It should be noted that coarse aggregate was not used in this study.