Title: Structural Bending Properties of Higher Strength Concrete

Author(s): S. E. Swartz, A. Nikaeen, H. D. Narayan Babu, N. Periyakaruppan, and T. M. E. Refai

Publication: Special Publication

Volume: 87

Issue:

Appears on pages(s): 147-178

Keywords: beams (supports); bending; high-strength concretes; modulus of elasticity; plain concrete; reinforced concrete; research; strains; stress block; stress-strain diagrams.

Date: 9/1/1985

Abstract:
Higher strength concrete which is defined to be that with uniaxial, 12000 psi compressive strength in the range of 6000 psi