Title: Rational Deformation Prediction of Prestressed Members

Author(s): Alex Aswad

Publication: Symposium Paper

Volume: 86

Issue:

Appears on pages(s): 263-282

Keywords: age; beams (supports); camber; creep properties; defor-mation; prestressed concrete; prestressing steels; prestress loss; pretensioning; roofs; shrinkage; structural analysis; viscoelas-ticity.

Date: 8/1/1985

Abstract:
age; beams (supports); camber; creep properties; defor-mation; prestressed concrete; prestressing steels; prestress loss; pretensioning; roofs; shrinkage; structural analysis; viscoelas-ticity.




  