Title: Design and Construction of Two-Way Slabs for Deflection Control

Author(s): A. Scanlon

Publication: Symposium Paper

Volume: 183

Issue:

Appears on pages(s): 145-161

Keywords: cracking; deflection control; design; slabs

DOI: 10.14359/5539

Date: 5/1/1999

Abstract:
Deflection control for two-way slab systems requires attention to both design and construction requirements. This paper discusses both aspects and provides a design example to illustrate how construction loads, cracking and time-dependent effects can be accounted for in slab deflection calculations.




  