Title: EV-01: Batching, Mixing, and Transportation of Ready-Mixed Concrete
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s):
Keywords: handling concrete
Date: 1/1/1992
Abstract:
Note: EV-01 is No Longer Available.
This video covers the recommended procedures for manufacturing and delivering ready-mixed concrete based on ASTM C94. It also goes through weighing all the different types of stationary and transit mixers, delivery vehicles, transit times and techniques, and control of the concrete at the job site. A short portion also covers inspection of the fresh concrete--typically the strength test results of a series of concrete cylinders.