Title: C-24: Durable Concrete

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 71

Keywords: durability

Date: 1/1/1993

Abstract:

Note: C-24 is No Longer Available.

Durable Concrete contains important information found in article on topics including long service life of concrete, design considerations for service life, research innovations for durable concrete, the use of fly ash, economic considerations, water and its role in concrete, concrete in a sulfate environment, the use of superplasticizers, effective curing on durability, shotcrete durability, and exposed aggregate concrete.




  