Title:
C-17: High Strength Concrete
Author(s):
Publication:
Technical Documents
Volume:
Issue:
Appears on pages(s):
96
Keywords:
high-strength concrete
DOI:
Date:
1/1/1992
Abstract:
This compilation consists of 18 technical papers and articles on the subject. An additional section on Letters to the Editor from Concrete International magazine is also included. A sampling of the subjects includes research, high PCS, production and delivery, new mineral admixtures, influencing principles and factors, long-term characteristics, and pumping methods.