In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: 506R-90 (Reapproved 1995): Guide to Shotcrete
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 41
Keywords: shotcreting
Date: 10/10/1995
Abstract:Note: A newer version of this document exists. This document was replaced by 506R-05. Recommendations are given on the applicability of shotcrete to different types of construction, material requirements, and application procedures. Equipment requirements are given for both the dry mix and wet mix processes. The testing of shotcrete is covered in detail. Emphasis is placed on the competence of the application crew.
Note: A newer version of this document exists. This document was replaced by 506R-05.