Pozzolanic Reactivity of Supplementary Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pozzolanic Reactivity of Supplementary Cementitious Materials

Author(s): Keshav Bharadwaj, O. Burkan Isgor, and W. Jason Weiss

Publication: Materials Journal

Volume: 120

Issue: 4

Appears on pages(s): 63-76

Keywords: pozzolanic reactivity test (PRT); reactivity; supplementary cementitious materials (SCMs); thermodynamic modeling

DOI: 10.14359/51738817

Date: 7/1/2023

Abstract:
As the number of potential supplementary cementitious materials (SCMs) increase, there is a need to determine their reactivity. Most recent methods to assess pozzolanic reactivity are based on measuring certain outputs such as heat release (Q), calcium hydroxide (CH) consumption, and nonevaporable water. This paper uses thermodynamic modeling to aid in the interpretation of these tests and the quantification of reactivity. It is shown that pozzolanic reactivity should be interpreted based on the SCM type. The presence of sulfates and carbonates during reactivity quantification alter the reaction of the Al2O3 phases, making the interpretation of the reactivity test results challenging. The reactivity of commercial SCMs should be interpreted specific to the type of SCM as described by ASTM International/AASHTO. A proposed interpretation for commercial SCMs is provided in this paper.

Related References:

1. Thomas, M., Supplementary Cementing Materials in Concrete, CRC Press, Boca Raton, FL, 2013, 210 pp.

2. Bredy, P.; Chabannet, M.; and Pera, J., “Microstructure and Porosity of Metakaolin Blended Cements,” MRS Online Proceedings Library Archive, V. 137, 1988.

3. Bharadwaj, K.; Ghantous, R. M.; Sahan, F. N.; Isgor, B. O.; and Weiss, J., “Predicting Pore Volume, Compressive Strength, Pore Connectivity, and Formation Factor in Cementitious Pastes Containing Fly Ash,” Cement and Concrete Composites, V. 122, Paper No. 104113, 2021.

4. Lothenbach, B.; Scrivener, K.; and Hooton, R. D., “Supplementary Cementitious Materials,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1244-1256. doi: 10.1016/j.cemconres.2010.12.001

5. Poon, C.-S.; Kou, S.; and Lam, L., “Compressive Strength, Chloride Diffusivity and Pore Structure of High Performance Metakaolin and Silica Fume Concrete,” Construction and Building Materials, V. 20, No. 10, 2006, pp. 858-865. doi: 10.1016/j.conbuildmat.2005.07.001

6. Pepper, L., and Mather, B., “Effectiveness of Mineral Admixtures in Preventing Excessive Expansion of Concrete Due to Alkali-Aggregate Reaction,” American Society for Testing Materials - Proceedings, Philadelphia, PA, 1959.

7. Thomas, M., “The Effect of Supplementary Cementing Materials on Alkali-Silica Reaction: A Review,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1224-1231. doi: 10.1016/j.cemconres.2010.11.003

8. Suraneni, P.; Azad, V. J.; Isgor, B. O.; and Weiss, W. J., “Calcium Oxychloride Formation in Pastes Containing Supplementary Cementitious Materials: Thoughts on the Role of Cement and Supplementary Cementitious Materials Reactivity,” RILEM Technical Letters, V. 1, 2016, pp. 24-30. doi: 10.21809/rilemtechlett.2016.7

9. Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, W. J., “Deicing Salts and Durability of Concrete Pavements and Joints,” Concrete International, V. 38, No. 4, Apr. 2016, pp. 48-54.

10. Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, W. J., “Use of Fly Ash to Minimize Deicing Salt Damage in Concrete Pavements,” Transportation Research Record: Journal of the Transportation Research Board, V. 2629, No. 1, 2017, pp. 24-32. doi: 10.3141/2629-05

11. Whatley, S. N.; Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, J., “Mitigation of Calcium Oxychloride Formation in Cement Pastes Using Undensified Silica Fume,” Journal of Materials in Civil Engineering, ASCE, V. 29, No. 10, Paper No.04017198, 2017. doi: 10.1061/(ASCE)MT.1943-5533.00020

12. Juenger, M. C.; Snellings, R.; and Bernal, S. A., “Supplementary Cementitious Materials: New Sources, Characterization, and Performance Insights,” Cement and Concrete Research, V. 122, 2019, pp. 257-273. doi: 10.1016/j.cemconres.2019.05.008

13. Butalia, T. S., “Beneficial Use of Ponded Fly Ash in Structural Concrete,” UKIERI Concrete Congress Key Note Address, Jalandhar: Dr. B. R. Ambedkar National Institute of Technology, Jalandhar, Punjab, India, 2019.

14. Innocenti, G.; Benkeser, D. J.; Dase, J. E.; Wirth, X.; Sievers, C.; and Kurtis, K. E., “Beneficiation of Ponded Coal Ash through Chemi-Mechanical Grinding,” Fuel, V. 299, Paper No.120892, 2021.

15. Clavier, K. A.; Paris, J. M.; Ferraro, C. C.; and Townsend, T. G., “Opportunities and Challenges Associated with Using Municipal Waste Incineration Ash as a Raw Ingredient in Cement Production—A Review,” Resources, Conservation and Recycling, V. 160, Paper No.104888, 2020.

16. Bahurudeen, A.; Kanraj, D.; Gokul Dev, V.; and Santhanam, M., “Performance Evaluation of Sugarcane Bagasse Ash Blended Cement in Concrete,” Cement and Concrete Composites, V. 59, 2015, pp. 77-88. doi: 10.1016/j.cemconcomp.2015.03.004

17. Bahurudeen, A.; Marckson, A.; Kishore, A.; and Santhanam, M., “Development of Sugarcane Bagasse Ash Based Portland Pozzolana Cement and Evaluation of Compatibility with Superplasticizers,” Construction and Building Materials, V. 68, 2014, pp. 465-475. doi: 10.1016/j.conbuildmat.2014.07.013

18. Bahurudeen, A., and Santhanam, M., “Influence of Different Processing Methods on the Pozzolanic Performance of Sugarcane Bagasse Ash,” Cement and Concrete Composites, V. 56, 2015, pp. 32-45. doi: 10.1016/j.cemconcomp.2014.11.002

19. PCA, Design and Control of Concrete Mixtures, Portland Cement Association, Skokie, IL, 2012, 459 pp.

20. Bharadwaj, K.; Isgor, B. O.; Weiss, J. W.; Chopperla, K. S. T.; Choudhary, A.; Vasudevan, G.; Glosser, D.; Ideker, J.; and Trejo, D., “A New Mixture Proportioning Method for Performance-Based Concrete,” ACI Materials Journal, V. 119, No. 2, Mar. 2022, pp. 207-220.

21. Mehta, P. K., and Monteiro, P. J., Concrete: Microstructure, Properties and Materials, McGraw Hill Professional, New Delhi, India, 2006, 675 pp.

22. Taylor, H. F., Cement Chemistry, Thomas Telford, London, UK, 1997, 459 pp.

23. Glosser, D.; Choudhary, A.; Isgor, O. B.; and Weiss, W. J., “Investigation of Reactivity of Fly Ash and Its Effect on Mixture Properties,” ACI Materials Journal, V. 116, No. 4, July 2019, pp. 193-200. doi: 10.14359/51716722

24. Glosser, D.; Suraneni, P.; Isgor, O. B.; and Weiss, W. J., “Estimating Reaction Kinetics of Cementitious Pastes Containing Fly Ash,” Cement and Concrete Composites, V. 112, Paper No. 103655, 2020.

25. ASTM C618-19, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2019.

26. AASHTO M 295, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” American Association of State Highway and Transportation Officials (AASHTO), Washington, DC, 2019.

27. EN 206-1, “Concrete—Part 1: Specification, Performance, Production and Conformity,” European Committee for Standardization, Brussels, Belgium, 2000.

28. Papadakis, V. G., and Tsimas, S., “Supplementary Cementing Materials in Concrete: Part I: Efficiencya Design,” Cement and Concrete Research, V. 32, No. 10, 2002, pp. 1525-1532. doi: 10.1016/S0008-8846(02)00827-X

29. Glosser, D.; Suraneni, P.; Isgor, O. B.; and Weiss, W. J., “Using Glass Content to Determine the Reactivity of Fly Ash for Thermodynamic Calculations,” Cement and Concrete Composites, V. 115, Paper No.103849, 2021.

30. Durdziński, P. T.; Dunant, C. F.; Haha, M. B.; and Scrivener, K. L., “A New Quantification Method Based on Sem-Eds to Assess Fly Ash Composition and Study the Reaction of Its Individual Components in Hydrating Cement Paste,” Cement and Concrete Research, V. 73, 2015, pp. 111-122. doi: 10.1016/j.cemconres.2015.02.008

31. EN 196-5, “Methods of Testing Cement—Part 5: Pozzolanicity Test for Pozzolanic Cement,” European Committee for Standardization, Brussels, Belgium, 2011.

32. Chapelle, J., “Attaque sulfo-calcique des laitiers et des pouzzolanes,” Imprimerie Centrale de l’Ortois-Orras, 1958, pp. 193-201.

33. Choudhary, A.; Bharadwaj, K.; Ghantous, R. M.; Isgor, B.; and Weiss, J., “Pozzolanic Reactivity Test of Supplementary Cementitious Materials,” ACI Materials Journal, V. 119, No. 2, Mar. 2022, pp. 255-268.

34. Thorstensen, R. T., and Fidjestol, P., “Inconsistencies in the Pozzolanic Strength Activity Index (SAI) for Silica Fume According To EN and ASTM,” Materials and Structures, V. 48, No. 12, 2015, pp. 3979-3990. doi: 10.1617/s11527-014-0457-6

35. Bentz, D. P.; Durán-Herrera, A.; and Galvez-Moreno, D., “Comparison of ASTM C311 Strength Activity Index Testing Versus Testing Based on Constant Volumetric Proportions,” Journal of ASTM International, V. 9, No. 1, 2011, pp. 1-7.

36. ASTM C1897-20, “Standard Test Method for Measuring the Reactivity of Supplementary Cementitious Materials by Isothermal Calorimetry and Bound Water Measurements,” ASTM International, West Conshohocken, PA, 2020.

37. Avet, F.; Snellings, R.; Alujas Diaz, A.; Ben Haha, M.; and Scrivener, K., “Development of a New Rapid, Relevant and Reliable (R-3) Test Method to Evaluate the Pozzolanic Reactivity of Calcined Kaolinitic Clays,” Cement and Concrete Research, V. 85, 2016, pp. 1-11. doi: 10.1016/j.cemconres.2016.02.015

38. Snellings, R., and Scrivener, K. L., “Rapid Screening Tests for Supplementary Cementitious Materials: Past and Future,” Materials and Structures, V. 49, No. 8, 2016, pp. 3265-3279. doi: 10.1617/s11527-015-0718-z

39. Bharadwaj, K.; Isgor, B. O.; and Weiss, J. W., “A Simplified Approach to Determine the Pozzolanic Reactivity of Commercial Supplementary Cementitious Materials,” Concrete International, V. 44, No. 1, Jan. 2022, pp. 27-32.

40. Azad, V. J.; Suraneni, P.; Trejo, D.; Weiss, W. J.; and Isgor, O. B., “Thermodynamic Investigation of Allowable Admixed Chloride Limits in Concrete,” ACI Materials Journal, V. 115, No. 5, Sept. 2018, pp. 727-738. doi: 10.14359/51702349

41. Bharadwaj, K.; Chopperla, K. S. T.; Choudhary, A.; Glosser, D.; Ghantous, R. M.; Vasudevan, G.; Ideker, J. H.; Isgor, B.; Trejo, D.; and Weiss, J. W., “Caltrans: Impact of the Use of Portland-Limestone Cement on Concrete Performance as Plain or Reinforced Material—Final Report,” Oregon State University, Corvallis, OR, 320 pp.

42. Bharadwaj, K.; Glosser, D.; Moradllo, M. K.; Isgor, O. B.; and Weiss, J., “Toward the Prediction of Pore Volumes and Freeze-Thaw Performance of Concrete Using Thermodynamic Modelling,” Cement and Concrete Research, V. 124, Paper No. 105820, 2019.

43. Bharadwaj, K.; Isgor, B. O.; and Weiss, J. W., “Supplementary Cementitious Materials in Portland Limestone Cements,” ACI Materials Journal, V. 119, No. 2, Mar. 2022, pp. 141-154.

44. Choudhary, A.; Ghantous, R. M.; Bharadwaj, K.; Opdahl, O. H.; Isgor, B. O.; and Weiss, J. W., “Electrical and Transport Properties of Cement Mortar Made Using Portland Limestone Cement,” Advances in Civil Engineering Materials, V. 11, No. 1, 2022, pp. 263-279. doi: 10.1520/ACEM20210119

45. Glosser, D.; Azad, V. J.; Suraneni, P.; Isgor, B.; and Weiss, J., “Extension of Powers-Brownyard Model to Pastes Containing Supplementary Cementitious Materials,” ACI Materials Journal, V. 116, No. 5, Sept. 2019, pp. 205-216. doi: 10.14359/51714466

46. Suraneni, P., and Weiss, J., “Examining the Pozzolanicity of Supplementary Cementitious Materials Using Isothermal Calorimetry and Thermogravimetric Analysis,” Cement and Concrete Composites, V. 83, 2017, pp. 273-278. doi: 10.1016/j.cemconcomp.2017.07.009

47. Glosser, D.; Isgor, O. B.; and Weiss, W. J., “Non-Equilibrium Thermodynamic Modeling Framework for Ordinary Portland Cement/Supplementary Cementitious Material Systems,” ACI Materials Journal, V. 117, No. 6, Nov. 2020, pp. 111-123.

48. Ramanathan, S., “Reactivity of Supplementary Cementitious Materials in Model Systems and Cementitious Pastes,” PhD thesis, University of Miami, Miami, FL, 2021.

49. Ramanathan, S.; Croly, M.; and Suraneni, P., “Comparison of the Effects that Supplementary Cementitious Materials Replacement Levels Have on Cementitious Paste Properties,” Cement and Concrete Composites, V. 112, Paper No. 103678, 2020.

50. Ramanathan, S.; Kasaniya, M.; Tuen, M.; Thomas, M. D.; and Suraneni, P., “Linking Reactivity Test Outputs to Properties of Cementitious Pastes Made with Supplementary Cementitious Materials,” Cement and Concrete Composites, V. 114, Paper No. 103742, 2020.

51. Ramanathan, S.; Moon, H.; Croly, M.; Chung, C.-W.; and Suraneni, P., “Predicting the Degree of Reaction of Supplementary Cementitious Materials in Cementitious Pastes Using a Pozzolanic Test,” Construction and Building Materials, V. 204, 2019, pp. 621-630. doi: 10.1016/j.conbuildmat.2019.01.173

52. Ramanathan, S.; Perumal, P.; Illikainen, M.; and Suraneni, P., “Mechanically Activated Mine Tailings for Use as Supplementary Cementitious Materials,” RILEM Technical Letters, V. 6, 2021, pp. 61-69. doi: 10.21809/rilemtechlett.2021.143

53. Ramanathan, S.; Pestana, L. R.; and Suraneni, P., “Reaction Kinetics of Supplementary Cementitious Materials in Reactivity Tests,” Cement, Paper No. 100022, 2022.

54. Ramanathan, S.; Suraneni, P.; Wang, Y.; Shan, H.; Hajibabaee, A.; and Weiss, J., “Combining Reactivity Test, Isothermal Calorimetry, and Compressive Strength Measurements to Study Conventional and Alternative Supplementary Cementitious Materials,” Proceedings of the International Conference of Sustainable Production and Use of Cement and Concrete, 2020, pp. 445-454.

55. Suraneni, P.; Hajibabaee, A.; Ramanathan, S.; Wang, Y.; and Weiss, J., “New Insights from Reactivity Testing of Supplementary Cementitious Materials,” Cement and Concrete Composites, V. 103, 2019, pp. 331-338. doi: 10.1016/j.cemconcomp.2019.05.017

56. Suraneni, P., and Ramanathan, S., “Reactivity of Tested SCMs,” personal communication sent to W. J. Weiss, K. Bharadwaj, and B. O. Isgor, 2020.

57. Ramanathan, S.; Tuen, M.; and Suraneni, P., “Influence of Supplementary Cementitious Material and Filler Fineness on Their Reactivity in Model Systems and Cementitious Pastes,” Materials and Structures, V. 55, No. 5, 2022, 25 pp. doi: 10.1617/s11527-022-01980-2

58. Moradllo, M. K.; Chung, C.-W.; Keys, M. H.; Choudhary, A.; Reese, S. R.; and Weiss, W. J., “Use of Borosilicate Glass Powder in Cementitious Materials: Pozzolanic Reactivity and Neutron Shielding Properties,” Cement and Concrete Composites, V. 112, Paper No. 103640, 2020.

59. Burroughs, J. F., “Influence of Chemical and Physical Properties of Poorly-Ordered Silica on Reactivity and Rheology of Cementitious Materials,” PhD thesis, Purdue University, West Lafayette, IN, 2019.

60. Isgor, B.; Ideker, J.; Trejo, D.; Weiss, J.; Bharadwaj, K.; Choudhary, A.; Teja, C. K. S.; Glosser, D.; and Vasudevan, G., “Development of a Performance-Based Mixture Proportioning Procedure for Concrete Incorporating Off-Spec Fly Ash,” Energy Power Research Institute (EPRI), Palo Alto, CA, 78 pp.

61. Kim, T., and Olek, J., “Effects of Sample Preparation and Interpretation of Thermogravimetric Curves on Calcium Hydroxide in Hydrated Pastes and Mortars,” Transportation Research Record: Journal of the Transportation Research Board, V. 2290, No. 1, 2012, pp. 10-18. doi: 10.3141/2290-02

62. Lothenbach, B.; Matschei, T.; Möschner, G.; and Glasser, F. P., “Thermodynamic Modelling of the Effect of Temperature on the Hydration and Porosity of Portland Cement,” Cement and Concrete Research, V. 38, No. 1, 2008, pp. 1-18. doi: 10.1016/j.cemconres.2007.08.017

63. Lothenbach, B., and Winnefeld, F., “Thermodynamic Modelling of the Hydration of Portland Cement,” Cement and Concrete Research, V. 36, No. 2, 2006, pp. 209-226. doi: 10.1016/j.cemconres.2005.03.001

64. Kulik, D. A.; Wagner, T.; Dmytrieva, S. V.; Kosakowski, G.; Hingerl, F. F.; Chudnenko, K. V.; and Berner, U. R., “Gem-Selektor Geochemical Modeling Package: Revised Algorithm and GEMS3K Numerical Kernel for Coupled Simulation Codes,” Computational Geosciences, V. 17, No. 1, 2013, pp. 1-24.

65. Lothenbach, B.; Kulik, D. A.; Matschei, T.; Balonis, M.; Baquerizo, L.; Dilnesa, B.; Miron, G. D.; and Myers, R. J., “Cemdata 18: A Chemical Thermodynamic Database for Hydrated Portland Cements and Alkali-Activated Materials,” Cement and Concrete Research, V. 115, 2019, pp. 472-506. doi: 10.1016/j.cemconres.2018.04.018

66. Gosselin, C., “Microstructural Development of Calcium Aluminate Cement Based Systems with and without Supplementary Cementitious Materials,” PhD thesis, Swiss Federal Institute of Technology Lausanne, Lausanne, Switzerland, 234 pp.

67. Choudhary, A., “The Pozzolanic Reactivity Test and the Properties of Portland Limestone Cement,” PhD thesis, Oregon State University, Corvallis, OR, 2021.

68. NIST, “NIST Chemistry WebBook,” National Institute of Standards and Technology (NIST), Gaithersburg, MD, 2021, doi: 10.18434/T4D30310.18434/T4D303

69. de Silva, P., and Glasser, F. P., “Phase Relations in the System CaO Al2O3 SiO2 H2O Relevant to Metakaolin-Calcium Hydroxide Hydration,” Cement and Concrete Research, V. 23, No. 3, 1993, pp. 627-639. doi: 10.1016/0008-8846(93)90014-Z

70. AASHTO M 307, “Standard Specification for Silica Fume Used in Cementitious Mixtures,” American Association of State Highway and Transportation Officials, Washington, DC, 2013.

71. ASTM C1240-20, “Standard Specification for Silica Fume Used in Cementitious Mixtures,” ASTM International, West Conshohocken, PA, 2020.

72. Matschei, T.; Lothenbach, B.; and Glasser, F., “The AFM Phase in Portland Cement,” Cement and Concrete Research, V. 37, No. 2, 2007, pp. 118-130. doi: 10.1016/j.cemconres.2006.10.010

73. ASTM C989/C989M-18a, “Standard Specification for Slag Cement for Use in Concrete and Mortars,” ASTM International, West Conshohocken, PA, 2018.