ASTM A955/A955M-20a, "Standard Specification for Deformed and Plain Stainless-Steel Bars for Concrete Reinforcement."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM A955/A955M-20a, "Standard Specification for Deformed and Plain Stainless-Steel Bars for Concrete Reinforcement."

Author(s): ASTM Subcommittee A01.05 on Steel Reinforcement

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/A0955_A0955M-20A

Date: 5/1/2020

Abstract:
This specification covers deformed and plain stainless steel bars for concrete reinforcement proposed to be used in applications requiring corrosion resistance or controlled magnetic permeability. For each specimen, one tension test, one bend test, if required, and one set of dimensional property tests shall be made. For martensitic materials, two hardness tests shall be performed per lot of material. If the results of the test fail to meet the specified minimum requirements, a retest shall be permitted on two random specimens for each original tension specimen failure from the lot. If a specimen fails a bend test due to reasons other than mechanical or flaws, a retest shall be permitted on two random specimens from the same lot.