Title: Interaction between Shrinkage Mitigating Materials to Reduce Shrinkage Cracking in Concrete Bridge Decks

Author(s): Iman Mehdipour

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
Measuring elements on the order of 10-6 in/in, typical for concrete shrinkage, in a laboratory setting can be difficult. In situ testing of concrete shrinkage has the added complication of variations in temperature and humidity. This discussion will discuss cost effective measures to ensure shrinkage compensation in the field.




  