Title: Groundbreaking Technologies: Carbon Capture and Storage (CCS)

Author(s): Cariaga

Publication: Web Session

Volume: ws_F21_Cariaga.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
Some CO2 emissions during cement production process are inevitable and cannot be eliminated using established techniques of clinker substitution and alternative fuels. Therefore, new approaches are needed to deal with this CO2 in order to reach our vision of carbon-neutral concrete. Carbon capture technologies provide a solution to ultimately reduce hard-to abate emissions.