APPLICATION OF ANTI-WASHOUT UNDERWATER CONCRETE TO REPAIR OF AN UNDERWATER STRUCTURE

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: APPLICATION OF ANTI-WASHOUT UNDERWATER CONCRETE TO REPAIR OF AN UNDERWATER STRUCTURE

Author(s): Prachark Premchit, Chalermchai Wanichlamlert, Pitisan Krammart, Somnuk Tangtermsirikul

Publication: TCA

Volume:

Issue: Vol. 5 No. 1 (2017): January 2017 - June 2017

Appears on pages(s):

Keywords: Anti-washout admixture, underwater concrete, underwater structures

DOI:

Date: 6/30/2017

Abstract:
A project of an underwater concrete structure repair using an innovation of anti-washout underwater concrete is presented in this paper. Presented in this paper are the development concept of the anti-washout underwater concrete and its application for solving specific problems in this repair and construction works. The results showed that the developed mix proportion of the underwater concrete together with the procedures, methods and techniques of underwater concrete pouring in marine environment with wind waves, can be applied to the Pilot Station Building Renovation Project in Samut Prakarn Province. The underwater concrete had good anti-washout resistance in fresh state and did not allow blending with outer water. This success leads to the new technique for efficient concrete pouring in underwater condition.