Title: Shotcrete Incorporated into ACI 318-19 Building Code

Author(s): Charles Hanskat, Terence C. Holland, and Bruce A. Suprenant

Publication: Concrete International

Volume: 41

Issue: 12

Appears on pages(s): 31-35

Keywords: committee, provision, mix, standard

DOI:

Date: 12/1/2019

Abstract:
Shotcrete has been incorporated into the International Building Code (IBC) for many years but was not expressly covered in the ACI 318 Code. Conversations between ACI and International Code Council staff indicated that it would be possible to delete the shotcrete provisions from the IBC upon satisfactory incorporation of shotcrete into the ACI 318 Code. Thus, ACI Subcommittees 318-A and 318-B worked for 5 years to successfully include shotcrete into ACI 318-19.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer