International Concrete Abstracts Portal

  


Title: Shear Crack Prediction in Shallow Reinforced Concrete Beams Using a Nonlinear Approach

Author(s): AlaaEldin Abouelleil and Hayder A. Rasheed

Publication: Structural Journal

Volume: 116

Issue: 6

Appears on pages(s): 153-163

Keywords: cracked concrete; diagonal tension cracks; shear-flexure cracks; shear stress analysis

DOI: 10.14359/51716809

Date: 11/1/2019

Abstract:
This study was conducted because of the lack of an existing theory to accurately predict diagonal tension cracking in shallow reinforced concrete beams. A rational approach is followed to numerically derive the shear stress profile across the depth of the section in cracked beams based on the smeared crack approach. Furthermore, the determined shear stress distribution coupled with the normal axial stress distribution are used to predict the principal stress variation across the depth and along the shear span using the standard Mohr’s circle. Following a biaxial stress cracking criterion, the likely diagonal tension cracks along their orientation profile are predicted.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer