Title: It Is All on the Contractors

Author(s): Carl Larosche

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 1/2/2019

Abstract:
The failure concrete repairs is largely the result of poor execution of the design details by contractors. The consistent poor execution of repair details creates the situations where repairs can fail in-service well before the expected service life is reached.




  