Title:
Chemistry Composition and Properties of Sulfated Cements
Author(s):
Krivoborodov Yury R., Samchenko S.V., and Kouznetsova T.V.
Publication:
Symposium Paper
Volume:
326
Issue:
Appears on pages(s):
27.1-27.6
Keywords:
sulfated clinkers, mineralogical composition, strength, expansion, range of application
DOI:
10.14359/51711009
Date:
8/10/2018
Abstract:
The paper presents the compositions and properties of sulfated clinkers; and, the cements based upon them. The conditions of formation of sulfated minerals such as calcium sulfoaluminate, sulfoferrite and sulfoalumio-ferrite are considered. The main physical and chemical characteristics of sulfated minerals are presented. Tech-nological peculiarities of production of clinkers, which have sulfated minerals, are studied. The properties of cements that are based on various sulfated clinkers are shown. Consideration is given to the possibilities of us-ing these clinkers for production of expanding, self-stressing, rapid-setting, fast hardening, corrosion-resistant, and oil-well cements. Examples of their usage both in construction and in other industries is discussed.
Related References:
1. Ragozina?.?. The interaction of sulfate with calcium aluminates at a temperature 12000C, Journal of Applied Chemistry, v.30, ?11, 1957, pp. 1682-1688.
2. Klein A. and Troxell G.E. Studies of Calcium Sulfoaluminate Admixures for Expansive Cements, Pros. ASTM, v.58, 1958,pp.986-1008.
3. Budnikov P.P., Kuznetsova I.P.The role of calcium sulphate in obtaining rapid hardening belite cement on the basis of low-grade bauxite, Works of.D..Mendeleev Institute of Chemical Technology, vol.36, 1961, pp. 129-132.
4. Halstead P.E. and Moore A.E. The composition and Crystallography of an Anhydrous Calcium Aluminosul-fate occuring in Expending Cements, Journ.App.Chemistry, 1972,v.12,p.417.
5. Kouznetsova T.V. Alumina and sulphoaluminate cements, Moscow, Strojizdat, 1986, 206 p.
6. Kurdowski, W., George, C.M., Sorrentino, F.P. Special cements. 8th International Congress on the Chemistry of Cement, Rio de Janeiro (Brazil) 22-27 September 1986, v.1, 292-318,.
7. A.P.Osokin , Y.R.Krivoborodov, S.V.Samchenko Expansive and non-shrinkage sulphomineral cements // 11th International Congress on the Chemistry of Cement (ICCC). Durban, South Africa, 2003, pp. 2083-2088.
8. Krivoborodov Y.R., Spizyn V.V., Klusov V.A. Oil-well cements for low temperature, Moscow, Publisher Mendeleev University of Chemical Technology, 2002, 125 p.
9. Samchenko S.V. Sulphated calcium alumoferrites and cement on their base, Moscow, Publisher Mendeleev University of Chemical Technology, 2005, 154 p.
10. Berekta, J. et al. Hydraulic behaviour of calcium sulfoaluminate-based cement derived from industrial pro-cess, Cement and Concrete Research, 26, 1993, pp.1673-1682.
11. Marroccoli, M., Montagnaro, F., Nobili, M., Telesca, A., Valenti, G. L., Synthesis, hydrationproperties and environmentally friendly features of calcium sulfoaluminate cements, 12th InternationalCongress on the Chemis-try of Cement, Montreal (Canada) 8-13 July 2007, W3, 11.2
12. Kouznetsova T.V., Krivoborodov Y.R., Samchenko S.V., Burlov I.Y. Special cements on base sulphoalumi-nate clinker, 13 International Congress on the Chemistry of Cement, Madrid (Spain) 3-8 July, 2011, v3,p. 198.
13. Muzhen, S., Yanmou, W., Zhang, L., Dedong, L., Preliminary study on the durability of sufo/ferroaluminate cements. 10th International Congress on the Chemistry of Cement, Goteborg (Sweden) 3-8 July1997: Amarkai AB and Congrex Goteborg AB, 4iv029.
14. Taylor, H. F. W. Cement Chemistry. Academic Press, London (UK),1997, 395p.
15. Buzzi, L., Canonico, F., Telesca, A., Valenti, G.L., 2010. High-performance and low-CO2 cements based on calcium sulphoaluminate. Zement Kalk Gips International, 5,2010, pp. 39-45.