Title: ESTUDIOS Y ENSAYOS RELATIVOS A LA FATIGA, A LA RELAJACION Y A LA ADHERENCIA DE ARMADURAS PARA HORMIGON ARMADO Y HORMIGON PRETENSADO.

Author(s): Baus, R.

Publication: ACHE

Volume: 20

Issue: 93

Appears on pages(s): 41 -

Keywords:

Date: 1/8/1969

Abstract:


ACI International Partner, ACHE Spain, International Partner Access.